dc.creatorZanin, Henrique Soares-
dc.creator.Latteshttp://lattes.cnpq.br/8075409022069956por
dc.contributor.advisor1Haupt, William-
dc.contributor.advisor1Latteshttp://lattes.cnpq.br/3288923141358212por
dc.date.accessioned2024-03-19T12:34:22Z-
dc.date.issued2023-09-27-
dc.identifier.citationZANIN, Henrique Soares. Avaliação da influência de eletrodos e gases de proteção em juntas soldadas do aço LNE 600. 2023. 111 f. Dissertação (Mestrado em Projeto e Processos de Fabricação) - Universidade de Passo Fundo, Passo Fundo, RS, 2023.por
dc.identifier.urihttp://tede.upf.br:8080/jspui/handle/tede/2597-
dc.description.resumoEste trabalho avaliou o comportamento dos aços de alta resistência e baixa liga (ARBL) após a soldagem, devido à alteração das propriedades mecânicas do material quando submetido a este processo. Desta forma, os principais objetivos foram avaliar: a influência de diferentes eletrodos na resistência a tração; o comportamento da dureza na zona termicamente afetada, a influência que o eletrodo e os gases de proteção exercem na microestrutura, no tamanho ZTA e na resistência a fadiga dos aços ARBL soldados pelo processo GMAW, aplicados em componentes. Para a confecção das amostras foram utilizados três diferentes tipos de eletrodos: ER70S-6, ER110S-G e ER120S-G e dois tipos de gases Ar + 5% O2 e Ar + 15% CO2, tendo como material base o aço LNE600. Na soldagem, os parâmetros de tensão e corrente foram mantidos constantes conforme especificação de procedimento de soldagem. Os resultados dos ensaios de tração e microdureza, concluíram que a soldagem utilizando o eletrodo ER120S-G na combinação com Ar + 15% CO2, apresentou o melhor comportamento com uma tensão média de escoamento de 680 MPa e dureza média de 320 HV na região do metal de adição, a carga utilizada no ensaio de microdureza foi 0,2 Kgf. Na microdureza não houve diferença estatística significativa para as regiões de grão grosseiro e grão refinado. Nos ensaios de fadiga de alta carga e baixo ciclo o eletrodo ER120S-G combinado com Ar + 5% O2 apresentou a maior média com 162 mil ciclos com 60% da carga estática estipulada, demais combinações apresentaram médias de ciclos variando de 74 a 99 mil sendo estatisticamente iguais. Para a condição com carga de 50% da estipula em projeto apenas a combinação do eletrodo ER70S-6 com o gás O2 apresentou uma performance inferior aos demais com 93 mil ciclos, as demais combinações apresentaram ciclos entre 175 a 189 mil sendo estatisticamente iguais.por
dc.description.abstractThis work evaluated the behavior of high-strength, low-alloy steels (ARBL) after welding, due to the change in the mechanical properties of the material when subjected to this process. Therefore, the main objectives were to evaluate: the influence of different electrodes on tensile strength; the behavior of hardness in the thermally affected zone, the influence that the electrode and protective gases have on the microstructure, the ZTA size and the fatigue resistance of ARBL steels welded by the GMAW process, applied to components. To prepare the samples, three different types of electrodes were used: ER70S-6, ER110S-G and ER120S-G and two types of gases Ar + 5% O2 and Ar + 15% CO2, using LNE600 steel as the base material. During welding, the voltage and current parameters were kept constant according to the welding procedure specification. The results of the tensile and microhardness tests concluded that welding using the ER120S-G electrode in combination with Ar + 15% CO2, presented the best behavior with an average yield stress of 680 MPa and average hardness of 320 HV in the region of filler metal, the load used in the microhardness test was 0.2 Kgf. In microhardness there was no statistically significant difference for the coarse grain and refined grain regions. In high load and low cycle fatigue tests, the ER120S-G electrode combined with Ar + 5% O2 presented the highest average with 162 thousand cycles with 60% of the stipulated static load, other combinations presented cycle averages varying from 74 to 99 thousand being statistically equal. For the condition with a load of 50% of the design stipulation, only the combination of the ER70S-6 electrode with the O2 gas presented a lower performance than the others with 93 thousand cycles, the other combinations presented cycles between 175 and 189 thousand, being statistically equal.eng
dc.description.provenanceSubmitted by Franciele Silva (francielesilva@upf.br) on 2024-03-19T12:34:22Z No. of bitstreams: 1 2023HenriqueSoaresZanin.pdf: 13121959 bytes, checksum: a2ac3d94539259f375747371c8bb7c62 (MD5)eng
dc.description.provenanceMade available in DSpace on 2024-03-19T12:34:22Z (GMT). No. of bitstreams: 1 2023HenriqueSoaresZanin.pdf: 13121959 bytes, checksum: a2ac3d94539259f375747371c8bb7c62 (MD5) Previous issue date: 2023-09-27eng
dc.formatapplication/pdf*
dc.languageporpor
dc.publisherUniversidade de Passo Fundopor
dc.publisher.departmentInstituto de Tecnologia – ITECpor
dc.publisher.countryBrasilpor
dc.publisher.initialsUPFpor
dc.publisher.programPrograma de Pós-Graduação em Projeto e Processos de Fabricaçãopor
dc.rightsAcesso Abertopor
dc.subjectProcessos de fabricaçãopor
dc.subjectJuntas soldadaspor
dc.subjectFerramentaspor
dc.subjectAço - Soldagempor
dc.subject.cnpqENGENHARIAS::ENGENHARIA DE PRODUCAOpor
dc.titleAvaliação da influência de eletrodos e gases de proteção em juntas soldadas do aço LNE 600por
dc.typeDissertaçãopor
Appears in Collections:Programa de Pós-Graduação em Projeto e Processos de Fabricação

Files in This Item:
File Description SizeFormat 
2023HenriqueSoaresZanin.pdfDissertação Henrique Soares Zanin12.81 MBAdobe PDFView/Open ???org.dspace.app.webui.jsptag.ItemTag.preview???


Items in TEDE are protected by copyright, with all rights reserved, unless otherwise indicated.