Title: Comportamento de fratura de coroas cerâmicas à base de zircônia submetidas ao jateamento com diferentes tamanhos de partícula
???metadata.dc.creator???: Mosele, João Cézar 
???metadata.dc.contributor.advisor1???: Borba, Márcia
???metadata.dc.description.resumo???: O objetivo deste estudo in vitro foi investigar a carga de fratura e modo de falha de coroas cerâmicas à base zircônia tetragonal estabilizada por ítria (Y-TZP) submetidas ao jateamento de óxido de alumínio com diferentes tamanhos de partículas. Sessenta infraestruturas de Y-TZP (Vita Inceram YZ) foram confeccionadas utilizando a tecnologia CAD-CAM, e recobertas com a porcelana compatível (Vita VM9). As restaurações foram divididas aleatoriamente em três grupos (n=20), conforme o tamanho das partículas de óxido de alumínio utilizadas no jateamento: (GC) sem tratamento (controle); (G53) partículas de 53 μm; (G125) partículas de 125 μm. Todas as coroas foram jateadas com uma pressão de 0,25 MPa e distância de 10 mm, por 10 s. As restaurações foram cimentadas sobre um pilar de resina reforçada por fibra utilizando um cimento resinoso. Todas as coroas foram testadas até a fratura utilizando um pistão esférico de aço inoxidável, em água destilada a 37o, em uma máquina de ensaios universal. A superfície de fratura das restaurações foi analisada com um estereomicroscópio. A rugosidade de superfície foi avaliada utilizando um perfilômetro óptico (n=5). Os resultados foram avaliados estatisticamente com análise de variância de um fator (ANOVA) e teste de Tukey (=0,05). A confiabilidade das restaurações foi obtida através da análise de Weibull. O grupo G125 apresentou maior média de carga máxima de fratura que o grupo controle. Os valores de carga máxima de fratura foram semelhantes para o G125 e G53. Não houve diferença entre os grupos para os resultados de módulo de Weibull (m) e resistência característica (0). Não foi observada diferença estatística nos valores médios dos parâmetros de rugosidade entre os grupos experimentais. No geral, foi observado, aproximadamente, 40% de fraturas catastróficas e 60% de lascamento de porcelana, não existindo relação entre o modo de fratura e o grupo experimental. Concluiu-se que o tamanho de partícula não teve influência na carga máxima de fratura, modo de falha, confiabilidade e rugosidade de coroas de Y-TZP
Abstract: The objective of this study was to investigate the fracture load and failure mode of yttrium partially stabilized tetragonal zirconia polycrystalline ceramic (Y-TZP) prosthetic crowns subjected to sandblasting with alumina particles with different sizes. Sixty Y-TZP frameworks were produced using CAD-CAM technology (Vita Inceram YZ) and veneered with porcelain (Vita VM9). Crowns were randomly divided into three groups (n=20), according to the alumina particle size used for sandblasting: (GC) no treatment (control); (G53) 53 μm alumina particles; (G125) 125 μm alumina particles. Sandblasting was performed with 0.25 MPa pressure at 10 mm distance, for 10 s. Crowns were adhesively cemented over a resin glass-reinforced die. All crowns were loaded until fracture by a stainless steel sphere, in a 37o distilled water bath, using a universal testing machine. Fracture surfaces were analyzed with a stereomicroscope. Surface roughness was evaluated using an optical perfilometer (n=5). Results were statistically analyzed by ANOVA and Tukey s test (=0.05). Reliability was accessed through Weibull analysis. G125 showed higher mean fracture load than the control group. G125 and G53 presented similar fracture load values. There were no significant differences between groups for Weibull modulus (m) and characteristic strength (0). Roughness parameters were also similar among groups. It was observed, approximately, 40% of catastrophic failures and 60% of chipping. There was no relation between failure mode and experimental group. It was concluded that the particle size had no influence on the fracture load, failure mode, reliability and surface roughness of Y-TZP crowns
Keywords: Restauração (Odontologia)
Cerâmica odontológica
Materiais dentários
Restoration ( Dentistry)
Dental ceramics
Dental materials
???metadata.dc.subject.cnpq???: CNPQ::CIENCIAS DA SAUDE::ODONTOLOGIA
???metadata.dc.language???: por
???metadata.dc.publisher.country???: BR
Publisher: Universidade de Passo Fundo
???metadata.dc.publisher.initials???: UPF
???metadata.dc.publisher.department???: Ciências da Saúde e Ciências Biológicas
???metadata.dc.publisher.program???: Programa de Pós-Graduação em Odontologia
Citation: MOSELE, João Cézar. Comportamento de fratura de coroas cerâmicas à base de zircônia submetidas ao jateamento com diferentes tamanhos de partícula. 2014. 134 f. Dissertação (Mestrado em Ciências da Saúde e Ciências Biológicas) - Universidade de Passo Fundo, Passo Fundo, 2014.
???metadata.dc.rights???: Acesso Aberto
URI: http://10.0.217.128:8080/jspui/handle/tede/828
Issue Date: 19-Apr-2014
Appears in Collections:Programa de Pós-Graduação em Odontologia

Files in This Item:
File SizeFormat 
2014JoaoCezarMosele.pdf2.95 MBAdobe PDFView/Open ???org.dspace.app.webui.jsptag.ItemTag.preview???


Items in TEDE are protected by copyright, with all rights reserved, unless otherwise indicated.